Material Notes:
Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation sterilization, easily processedApplications: radiation-sterilizable medical and laboratory devicesPassed USP Class VI testing. All ingredients meet TSCA (US) and DSL (Canada).Description: Pro-fax PF531 radiation-resistant, high melt flow, controlled rheology polypropylene homopolymer resin is designed for injection molding. This resin resists yellowing and embrittlement after 5 Mrads of gamma radiation. However, since performance and appearance after radiation sterilization can be sensitive to design and processing choices, the users should verify performance in their application. It passed USP Class VI testing. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 27 g/10 min

@Load 2.16 kg,
Temperature 230 °C
27 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785A
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Modulus 0.810 GPa
117 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648