Physical Properties Metric English Comments
Melt Flow 1.10 - 122 g/10 min
1.10 - 122 g/10 min
Average value: 32.1 g/10 min Grade Count:26
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Melt Flow 1.10 - 11.0 g/10 min
1.10 - 11.0 g/10 min
Average value: 5.88 g/10 min Grade Count:9
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Melt Flow 1.10 - 50.0 g/10 min
1.10 - 50.0 g/10 min
Average value: 17.4 g/10 min Grade Count:3
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Melt Flow 1.10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4764A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.10 - 22.7 g/10 min
1.10 - 22.7 g/10 min
Average value: 3.63 g/10 min Grade Count:24
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Melt Flow 1.10 - 20.0 g/10 min
1.10 - 20.0 g/10 min
Average value: 5.68 g/10 min Grade Count:16
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a..
Melt Flow 1.10 - 26.0 g/10 min
1.10 - 26.0 g/10 min
Average value: 4.90 g/10 min Grade Count:13
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
Melt Flow 1.10 - 9.80 g/10 min
1.10 - 9.80 g/10 min
Average value: 4.93 g/10 min Grade Count:4
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..