Physical Properties Metric English Comments
Melt Flow 2.9 - 3.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 - 3.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1525J (T28F) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 2.9 - 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 - 3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1550J (T30S) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Reliance Industries Repol H029SG Polypropylene
REPOL Polypropylene H029SG is being manufactured using Unipol PP process, which combines the production efficiency of gas phase fluidized bed reactor with the high activity stereospecific catalyst s..
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Reliance Industries Repol H029SP Polypropylene
REPOL Polypropylene H029SP is being manufactured using Unipol PP process, which combines the production efficiency of gas phase fluidized bed reactor with the high activity stereospecific catalyst s..
Melt Flow 2.9 g/10 min
2.9 g/10 min
ISO 1133
Lucite International Elvakon® 4470 High Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Melt Flow 2.9 g/10 min
2.9 g/10 min
ASTM D1238G
Hannam Chemical Hanalac 710 ABS
Melt Flow 2.9 g/10 min
2.9 g/10 min
ASTM D1238G
Hannam Chemical Hanalac 775 ABS, Extrusion Grade
Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,..
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Kuraray SEPTON® S64 Soft Compound
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre..
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene
Features:Halogenated Forms:PelletsInformation provided by Multibase
Melt Flow 2.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Styrolution PS 6210/6211 HIPS
Great balance of rigidity and toughnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Appeel® 72D799 Sealing Resin
DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Melt Flow 2.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform H 2320 006 Q600 POM
Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470.
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flam™ 1502 PP Black Polypropylene
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont Elvax® 3550SBH Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3550SBH is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv..