Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.5 - 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 - 3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM 585 General Purpose Polystyrene Grade 585 is a high molecular weight, low melt-flow crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. It is also suited.. |
|||
Melt Flow | 2.9 - 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.9 - 3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1550J (T30S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 1.5 - 3.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
1.5 - 3.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Kazanorgsintez PC-003 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Melt Flow | 3.1 - 3.5 g/10 min @Load 2.61 kg, Temperature 190 °C |
3.1 - 3.5 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |
|||
Melt Flow | 2.5 - 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 - 3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Granulate; ISO 1133/H |
SYNTHOS Krasten® 152 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with.. |
|||
Melt Flow | 0.80 - 3.5 g/10 min | 0.80 - 3.5 g/10 min | |
Shandong Dongyue Shenzhou New Material Co DS603A Fluorinated Ethylene Propylene Dispersion (DS603A/B) Conformable with: Q/DYS 004-2007Fluorinated Ethylene Propylene concentrated dispersion is the copolymer of TFE and HFP, stabilized with non-ionic surfactant. It endow FEP products which can't be pr.. |
|||
Melt Flow | 2.8 - 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 - 3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Granulate; ISO 1133/H |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |