Hannam Chemical Hanalac 775 ABS, Extrusion Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac 775 ABS, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, name plates
Physical Properties Metric English Comments
Melt Flow 2.9 g/10 min
2.9 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Yield Strength 63.0 MPa
9140 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched 3.80 J/cm

@Thickness 3.17 mm
7.12 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 88.0 °C
190 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Flammability, UL94 HB
HB