Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Flam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Halogenated Forms:PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.8 MPa
2870 psi
ASTM D638
Elongation at Break 930 %
930 %
ASTM D638
Flexural Strength 18.8 MPa
2730 psi
ASTM D790
Flexural Modulus 0.696 GPa
101 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Gardner Impact 21.47 J
15.83 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
0.118 in
V-2
V-2
0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
Dielectric Strength 25.3 kV/mm
642 kV/in
ASTM D149
Copyright © lookpolymers.com All Rights Reserved