Polymer Property : Melt Flow = 40.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.112 - 40.0 g/10 min
0.112 - 40.0 g/10 min
Average value: 8.51 g/10 min Grade Count:239
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Melt Flow 3.00 - 40.0 g/10 min
3.00 - 40.0 g/10 min
Average value: 15.9 g/10 min Grade Count:36
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
Melt Flow 0.500 - 40.0 g/10 min
0.500 - 40.0 g/10 min
Average value: 8.85 g/10 min Grade Count:96
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Melt Flow 1.00 - 40.0 g/10 min
1.00 - 40.0 g/10 min
Average value: 18.4 g/10 min Grade Count:19
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Melt Flow 20.0 - 40.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20.0 - 40.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW009 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (300000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 10.0 - 40.0 g/10 min
10.0 - 40.0 g/10 min
Average value: 20.3 g/10 min Grade Count:3
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Melt Flow 0.700 - 40.0 g/10 min
0.700 - 40.0 g/10 min
Average value: 10.7 g/10 min Grade Count:131
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..