Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.700 - 53.5 g/10 min | 0.700 - 53.5 g/10 min | Average value: 18.2 g/10 min Grade Count:66 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |