Polymer Property : Melt Flow = 0.58 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.32 - 0.58 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.32 - 0.58 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem GM 7040 G HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..