Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applications include blow molded containers for packaging household and agricultural chemicals, particularly those that are strong stress crack-inducing reagents.Regulatory Status: L5332CP meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Specific recommendations for processing L5332CP can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 100% Igepal® 450 hour
450 hour
Bent Strip; ASTM D1693
Melt Flow 0.32 g/10 min
0.32 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
1% Secant Modulus 1230 MPa
179000 psi
ASTM D790
Tensile Impact 125 J/cm
235 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525