Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Viscosity | 410000 cP | 410000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2095-60AB Elastomer KE-2095-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Viscosity | 410000 cP @Temperature 260 °C |
410000 cP @Temperature 500 °F |
Melt Viscosity; DSM method |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 410000 cP @Shear Rate 300 1/s, Temperature 190 °C |
410000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 410000 - 2.25e+6 cP @Temperature 260 - 260 °C |
410000 - 2.25e+6 cP @Temperature 500 - 500 °F |
Average value: 888000 cP Grade Count:16 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Viscosity | 410000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
410000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |