Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 410000 - 2.25e+6 cP @Temperature 260 - 260 °C |
410000 - 2.25e+6 cP @Temperature 500 - 500 °F |
Average value: 888000 cP Grade Count:16 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |