Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 28000 cP | 28000 cP | Part B, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Viscosity | 28000 cP | 28000 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 280 (SEMI-GEL) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 280 SERIES SEMI-GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The.. |
|||
Viscosity | 28000 - 32000 cP @Temperature 25.0 °C |
28000 - 32000 cP @Temperature 77.0 °F |
Uncured |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Viscosity | 28000 - 130000 cP @Temperature 204 - 204 °C |
28000 - 130000 cP @Temperature 399 - 399 °F |
Average value: 83800 cP Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Viscosity | 28000 - 32000 cP @Temperature 25.0 °C |
28000 - 32000 cP @Temperature 77.0 °F |
Uncured |
Permabond TA4246 Toughened Acrylic Adhesive PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with .. |
|||
Viscosity | 28000 - 32000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
28000 - 32000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2100419D1 Copper Paste This product has been designed as a copper ink for use in termination and circuit printing on ceramic substrates. This product contains a glass frit so may not be suitable for internal electrodes. .. |
|||
Viscosity | 28000 cP | 28000 cP | |
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit.. |
|||
Viscosity | 28000 cP @Temperature 25.0 °C |
28000 cP @Temperature 77.0 °F |
Mixed (10 rpm) |
Tra-Con Tra-Bond FDA22 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-22 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini.. |
|||
Viscosity | 28000 cP @Temperature 25.0 °C |
28000 cP @Temperature 77.0 °F |
Mixed (10 rpm) |
Tra-Con Tra-Bond FDA22BK01 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-22BK01 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance. This two-part black adhesive is easily mixed, used and cured at .. |
|||
Viscosity | 28000 cP @Temperature 25.0 °C |
28000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s.. |
|||
Viscosity | 28000 cP @Temperature 204 °C |
28000 cP @Temperature 399 °F |
Melt; ASTM D1084-88 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
Viscosity | 28000 cP | 28000 cP | |
Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy Two component, heat curing, aluminum filled epoxy suitable for high temperature tooling and a readily machinable repair or construction material. Similar to Duralco™ 132, but with a maximum servic.. |
|||
Viscosity | 28000 cP | 28000 cP | |
ACC MM918 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Viscosity | 28000 cP | 28000 cP | catalyzed with Moldmaster Green |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 28000 cP | 28000 cP | catalyzed with Moldmaster Blue |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 28000 cP | 28000 cP | catalyzed with Moldmaster Red |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 28000 cP | 28000 cP | catalyzed with Moldmaster Purple |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 28000 cP | 28000 cP | dynamic |
Dow Corning 3112 BASE & 1 CATALYST General purpose silicone mold making rubber suited for the reproduction of objects with no deep undercuts or complex shapes. 3112 Base with 1 Catalyst is recommended for use with rigid polyurethane .. |
|||
Viscosity | 28000 cP | 28000 cP | dynamic |
Dow Corning 3120 RTV SILICONE RUBBER Two-part, red, condensation cure, moderate flow, high temperature performance, UL HB, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |
|||
Viscosity | 28000 cP | 28000 cP | dynamic |
Dow Corning 3112 RTV SILICONE RUBBER Moldmaking RTV Rubber; Potting and encapsulating of electrical/electronic productsInformation provided by Dow Corning |