Physical Properties Metric English Comments
Viscosity 28000 cP
28000 cP
Part B, RVT, #5, 2.5 rpm; TM R050-12
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Viscosity 28000 cP
28000 cP
Liquid State
Palm Labs Adhesives Turbo Fuse Series 280 (SEMI-GEL) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 280 SERIES SEMI-GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The..
Viscosity 28000 - 32000 cP

@Temperature 25.0 °C
28000 - 32000 cP

@Temperature 77.0 °F
Uncured
Permabond TA430 Acrylic Adhesive & Initiator
PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin..
Viscosity 28000 - 130000 cP

@Temperature 204 - 204 °C
28000 - 130000 cP

@Temperature 399 - 399 °F
Average value: 83800 cP Grade Count:4
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Viscosity 28000 - 32000 cP

@Temperature 25.0 °C
28000 - 32000 cP

@Temperature 77.0 °F
Uncured
Permabond TA4246 Toughened Acrylic Adhesive
PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with ..
Viscosity 28000 - 32000 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
28000 - 32000 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2100419D1 Copper Paste
This product has been designed as a copper ink for use in termination and circuit printing on ceramic substrates. This product contains a glass frit so may not be suitable for internal electrodes. ..
Viscosity 28000 cP
28000 cP
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit..
Viscosity 28000 cP

@Temperature 25.0 °C
28000 cP

@Temperature 77.0 °F
Mixed (10 rpm)
Tra-Con Tra-Bond FDA22 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-22 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini..
Viscosity 28000 cP

@Temperature 25.0 °C
28000 cP

@Temperature 77.0 °F
Mixed (10 rpm)
Tra-Con Tra-Bond FDA22BK01 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-22BK01 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance. This two-part black adhesive is easily mixed, used and cured at ..
Viscosity 28000 cP

@Temperature 25.0 °C
28000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive
TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s..
Viscosity 28000 cP

@Temperature 204 °C
28000 cP

@Temperature 399 °F
Melt; ASTM D1084-88
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane
Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo..
Viscosity 28000 cP
28000 cP
Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy
Two component, heat curing, aluminum filled epoxy suitable for high temperature tooling and a readily machinable repair or construction material. Similar to Duralco™ 132, but with a maximum servic..
Viscosity 28000 cP
28000 cP
ACC MM918 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Viscosity 28000 cP
28000 cP
catalyzed with Moldmaster Green
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Viscosity 28000 cP
28000 cP
catalyzed with Moldmaster Blue
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Viscosity 28000 cP
28000 cP
catalyzed with Moldmaster Red
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Viscosity 28000 cP
28000 cP
catalyzed with Moldmaster Purple
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Viscosity 28000 cP
28000 cP
dynamic
Dow Corning 3112 BASE & 1 CATALYST
General purpose silicone mold making rubber suited for the reproduction of objects with no deep undercuts or complex shapes. 3112 Base with 1 Catalyst is recommended for use with rigid polyurethane ..
Viscosity 28000 cP
28000 cP
dynamic
Dow Corning 3120 RTV SILICONE RUBBER
Two-part, red, condensation cure, moderate flow, high temperature performance, UL HB, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning
Viscosity 28000 cP
28000 cP
dynamic
Dow Corning 3112 RTV SILICONE RUBBER
Moldmaking RTV Rubber; Potting and encapsulating of electrical/electronic productsInformation provided by Dow Corning