Material Notes:
Moldmaking RTV Rubber; Potting and encapsulating of electrical/electronic productsInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc

@Temperature 25.0 °C
1.30 g/cc

@Temperature 77.0 °F
Viscosity 28000 cP
28000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Ultimate 4.83 MPa
700 psi
Elongation at Break 130 %
130 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+13 ohm-cm
4.20e+13 ohm-cm
Dielectric Constant 3.2

@Frequency 100000 Hz
3.2

@Frequency 100000 Hz
3.25

@Frequency 100 Hz
3.25

@Frequency 100 Hz
Dielectric Strength 21.5 kV/mm
545 kV/in
Dissipation Factor 0.0040

@Frequency 100000 Hz
0.0040

@Frequency 100000 Hz
0.030

@Frequency 100 Hz
0.030

@Frequency 100 Hz
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Color white
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved