Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 150 - 200 cP @Temperature 23.0 °C |
150 - 200 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Cast 100 3D Printing Polymer High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar. |
|||
Viscosity | 150 - 300 cP @Temperature 25.0 °C |
150 - 300 cP @Temperature 77.0 °F |
Uncured |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Viscosity | 150 cP | 150 cP | |
Resinlab® AR 1018 Conformal Coating Resinlab™ AR 1018 is a one-part low viscosity acrylic based conformal coating for electronic circuit boards. It possesses excellent flexibility and adhesion to many substrates. It provides excell.. |
|||
Viscosity | 150 cP | 150 cP | Fed Std Method 4287 |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |
|||
Viscosity | 150 - 450 cP | 150 - 450 cP | |
Huntsman DY 064 Epoxy Accelerator Mix Ratio with GY 6010 is 5.Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Tri (dimethylamino methyl) phenol (DMP-30). Dark red, low vi.. |
|||
Viscosity | 150 - 300 cP | 150 - 300 cP | |
Huntsman HY 847 Cycloaliphatic Amine Approx. H+ equivalent weight 75. Mix Ratio with GY 6010 is 40.Comments/Applications: Medium viscosity, high performance hardener for self-leveling flooring.Data provided by Ciba Specialty Chemical.. |
|||
Viscosity | 150 cP | 150 cP | |
Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 150 - 170 cP | 150 - 170 cP | |
Huntsman Matrimid 5292A Resin Color: YellowComments/Applications: 4,4 Bismaleimidodiphenylmethane. Use with Matrimid 5292B to optimize processing, toughness and performance.Data provided by Ciba Specialty Chemicals.Ciba Special.. |
|||
Viscosity | <= 150 cP @Temperature 25.0 °C |
<= 150 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E2 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | 150 - 300 cP @Temperature 125 °C |
150 - 300 cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Viscosity | 150 - 300 cP @Temperature 125 °C |
150 - 300 cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer Description: The Epolene E-14EP is a low molecular weight, low density, oxidized polyethylene powder. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Viscosity | 150 cP @Temperature 23.0 °C |
150 cP @Temperature 73.4 °F |
|
Master Bond UV10LV One Component, Low Viscosity UV Curable Adhesive Master Bond UV10LV is a one part UV type system for bonding, sealing and coating that features good optical clarity and physical properties as well as low viscosity. This combination of properties a.. |
|||
Viscosity | 150 cP | 150 cP | dynamic |
Dow Corning 806A RESIN Silicone binder resin for colored baking enamels for space heaters, stoves, etc. Used alone or blended with Dow Corning® 805 Resin to promote intermediate hardness.Information provided by Dow Corni.. |
|||
Viscosity | 150 cP | 150 cP | dynamic |
Dow Corning H-10 ANTIFOAM EMULSION 10 percent active, water dilutable silicone emulsion designed to control foam in water based industrial processes.Information provided by Dow Corning |
|||
Viscosity | 150 cP | 150 cP | dynamic |
Dow Corning SYL-OFF® SL 2 CROSSLINKER Information provided by Dow Corning |
|||
Viscosity | 150 - 250 cP @Temperature 23.0 °C |
150 - 250 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th.. |
|||
Viscosity | 150 - 300 cP @Temperature 23.0 °C |
150 - 300 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
Viscosity | 150 cP | 150 cP | |
BASF Lupranate® 224 Isocyanate Description: Lupranate® 224 is a special medium viscosity polymeric MDI containing a high amount of 2,4'-diphenylmethane diisocyanate. The high 2,4'-MDI content will allow for better flow and lon.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, QM CAT 135 |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Purple |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Green |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Red |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 - 250 cP | 150 - 250 cP | |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 150 - 210 cP @Temperature 25.0 °C |
150 - 210 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-28 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyether-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for p.. |
|||
Viscosity | 150 - 300 cP @Temperature 25.0 °C |
150 - 300 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PE-210 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyester-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for .. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Purple |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 - 220 cP | 150 - 220 cP | |
Dow PAPI™ 27 Polymeric MDI PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,.. |
|||
Viscosity | 150 cP @Temperature 80.0 °C |
150 cP @Temperature 176 °F |
|
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t.. |