Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 180 - 220 cP | 180 - 220 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 140 (200 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 140 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 150 - 220 cP | 150 - 220 cP | |
Dow PAPI™ 27 Polymeric MDI PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,.. |
|||
Viscosity | 140 - 220 cP | 140 - 220 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® G1726 M (SEBS) Linear Triblock Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |