Material Notes:
Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyester-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for producing microcellular elastomers. First it can be used for manufacturing shoe-soles.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Viscosity 150 - 300 cP

@Temperature 25.0 °C
150 - 300 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
NCO Content, wt% 20.5 - 21.5