Permabond HL138 Anaerobic Retaining Compound

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond HL138 Anaerobic Retaining Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which eliminates wear, erosion, and pitting. Permabond HL138 cures to a tough cross-linked plastic and provides excellent environmental and temperature resistance. Since Permabond® HL138 can fill up the inner space, shaft-hub assemblies can be made with a clearance fit and eliminates an expensive press fit, while actually increasing the push out force. Permabond® HL138 develops full strength in a few hours on a large variety of substrates and is used on high speed production lines. Features & Benefits: Simple one-part fast cure low viscosity system Excellent shear strength Good environmental resistance Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 150 - 300 cP

@Temperature 25.0 °C
150 - 300 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 16.0 MPa
2320 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Zinc, handling strength
10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Zinc, working strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Aluminum, handling strength
180 min

@Temperature 23.0 °C
3.00 hour

@Temperature 73.4 °F
M10 steel, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Aluminum, working strength
Descriptive Properties Value Comments
Appearance Green
Uncured
Maximum Gap Fill (mm) 0.127
Maximum Thread Size M20
Strength Retention 50% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 20
M10 steel, break
36
M10 steel, prevail
UV Fluorescence No
Uncured