Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Melt Index of Compound | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Melt Index of Compound | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Melt Index of Compound | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | |
Lushan AR-5 Nylon Toughener/PA Impact Modifier Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Melt Index of Compound | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Braskem INSPIRE™ 137 NA Performance Polypropylene Polymer INSPIRE™ 137 Performance polymer is an impact copolymer, primarily designed for film extrusion and suitable for blow molding where high mechanical properties are of the highest importance.INSPIRE 1.. |
|||
Melt Index of Compound | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |