Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexibility, and good stress cracking resistance –ESCR. Its easy processability also allows high molding productivity, thickness control, and excellent surface appearance. Trithene® SX 7010 resin exhibits good chemical resistance with wide range of chemicals and solvents at room temperature. This product complies with ASTM standard D1248-IA4.Applications: Semi-rigid small containers designed for packing of household products such as bleach, deodorant, cosmetics, or any aggressive or non-aggressive products. Toys.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.921 - 0.924 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Melt Index of Compound 0.80 - 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ASTM D2240
Tensile Strength at Break 12.5 MPa
1810 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
ASTM D3418
Vicat Softening Point 91.0 °C
196 °F
ASTM D1525
Processing Properties Metric English Comments
Mold Temperature 15.0 - 15.0 °C
59.0 - 59.0 °F
(close to)