Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.925 g/cc
0.925 g/cc
ASTM D792
Melt Index of Compound 0.80 g/10 min
0.80 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.0 MPa
1600 psi
machine direction; ASTM D882
13.1 MPa
1900 psi
transverse direction; ASTM D882
Elongation at Break 650 %
650 %
machine direction; ASTM D882
800 %
800 %
transverse direction; ASTM D882
Flexural Modulus 0.276 GPa
40.0 ksi
machine direction; ASTM D882
0.310 GPa
45.0 ksi
transverse direction; ASTM D882
Optical Properties Metric English Comments
Gloss 55 %
55 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 125 °C
257 °F
Users viewing this material also viewed the following: