Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
ASTM D955
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
ASTM D955
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Thickness 3.18 mm
0.017 - 0.019 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Linear Mold Shrinkage, Transverse 0.016 - 0.019 cm/cm
0.016 - 0.019 in/in
LATI Latigray 75/4-01 CX/45 PBT
Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L..
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Thickness 3.18 mm
0.017 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Linear Mold Shrinkage, Transverse 0.0090 - 0.019 cm/cm
0.0090 - 0.019 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.0090 - 0.019 cm/cm
0.0090 - 0.019 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.0090 - 0.019 cm/cm
0.0090 - 0.019 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.0060 - 0.019 cm/cm
0.0060 - 0.019 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Transverse 0.0060 - 0.019 cm/cm
0.0060 - 0.019 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Transverse 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ISO DIS 294-4
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ISO DIS 294-4
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.0080 - 0.019 cm/cm
0.0080 - 0.019 in/in
Flame Bar; ASTM D955
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..