Material Notes:
Description: High Impact Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.024 - 0.028 cm/cm
0.024 - 0.028 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-93
Elongation at Break 75 %
75 %
ISO 527-93
Flexural Strength 60.0 MPa
8700 psi
ISO 178-93
Flexural Modulus 1.90 GPa
276 ksi
ISO 178-93
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93