Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm @Time 86400 sec |
0.017 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Sim. To ISO 294-4 |
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | |
Eurotec® Tecomid® NA40 NL IH PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection PBT-MD30Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX P D72.1 Polyester-Elastomer, Shore D75 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 cm/cm | 0.017 in/in | MPC method |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |