Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00250 - 0.0135 cm/cm
0.00250 - 0.0135 in/in
Average value: 0.00644 cm/cm Grade Count:37
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0135 cm/cm
0.0095 - 0.0135 in/in
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0135 cm/cm
0.0095 - 0.0135 in/in
LATI Latilub 62-06GR PA6, Graphite Reinforced
Self-lubricating product based on Polyamide 6 (PA6). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Linear Mold Shrinkage, Transverse 0.010 - 0.0135 cm/cm
0.010 - 0.0135 in/in
LATI Latilub 62-10T PA6
Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced
Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latimass 66-04 D009 PBT
Specific density compound based on Polybutylene Terephthalate (PBT). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0135 cm/cm
0.0095 - 0.0135 in/in
ISO DIS 294-4
Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
LATI Latimass 52/11-04 D008 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Linear Mold Shrinkage, Transverse 0.010 - 0.0135 cm/cm
0.010 - 0.0135 in/in
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Linear Mold Shrinkage, Transverse 0.0115 - 0.0135 cm/cm
0.0115 - 0.0135 in/in
LATI Latilub 95-15T PSU, PTFE Filled
Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici ..