Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 66 GF 30 TS 002 PA66 reinforced with glass fiber, heat stabilized PA66 for injection molding, reinforced with 30 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying pa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | |
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | |
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | ISO 294-4 |
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0145 cm/cm | 0.0115 - 0.0145 in/in | |
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0145 cm/cm | 0.0115 - 0.0145 in/in | |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.014 cm/cm | 0.0115 - 0.014 in/in | |
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0145 cm/cm | 0.0115 - 0.0145 in/in | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0145 cm/cm | 0.0115 - 0.0145 in/in | |
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0145 cm/cm | 0.0115 - 0.0145 in/in | |
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.014 cm/cm | 0.0115 - 0.014 in/in | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | 1 hr @ 80°C, xflow; SABIC Method |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | annealed; ISO 294-4 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 cm/cm | 0.0115 in/in | LATI |
LATI LARPEEK 50 G/20 20% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.0115 - 0.0135 cm/cm | 0.0115 - 0.0135 in/in | |
LATI Latilub 95-15T PSU, PTFE Filled Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |