Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0210 cm/cm | 0.00100 - 0.0210 in/in | Average value: 0.00968 cm/cm Grade Count:124 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0210 cm/cm | 0.0100 - 0.0210 in/in | Average value: 0.0144 cm/cm Grade Count:14 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage, Transverse | 0.00900 - 0.0210 cm/cm | 0.00900 - 0.0210 in/in | Average value: 0.0153 cm/cm Grade Count:8 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage, Transverse | 0.00930 - 0.0210 cm/cm | 0.00930 - 0.0210 in/in | Average value: 0.0140 cm/cm Grade Count:5 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage, Transverse | 0.00620 - 0.0210 cm/cm | 0.00620 - 0.0210 in/in | Average value: 0.0156 cm/cm Grade Count:8 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |