Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0100 - 0.0227 cm/cm
0.0100 - 0.0227 in/in
Average value: 0.0139 cm/cm Grade Count:9
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..