Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8387 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D297 |
Greene Tweed Fluoroelastomer 931 FKM Fluoroelastomer 931 performs well in aggressive chemical where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 931 has a good fie.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D792 |
Haysite SDL® H400 Polyester Composite H400 is an advanced composite that combines high temperature resistant and high strength characteristics with static dissipative properties for use as wave and reflow solder pallets. SDL Grade H400.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D297, 15 |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D297, 15 |
Seals Eastern 5722A Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
Shinil Chemical SHINCON PPS Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | at 25°C |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | at 25°C |
Daikin DAI-EL G-901 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance.Information provided by Daikin Industries. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
Colorite Polymers 9855 Radiopaque Vinyl Compound Description: Colorite radiopaque compounds are available in a variety of hardness and opacifier type. These compounds are designed for use as radiopaque striping or to be extruded into catheter tubi.. |
|||
Specific Gravity | 1.84 - 1.88 g/cc | 1.84 - 1.88 g/cc | ASTM D792 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | |
Bulk Molding Compounds BMC 5338 Mineral Filled, Glass Reinforced Polyester BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ASTM D792 |
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled
(discontinued **)< XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and .. |
|||
Specific Gravity | 1.84 g/cc | 1.84 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |