Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name Quartz-Coat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F)
Physical Properties Metric English Comments
Specific Gravity 1.84 g/cc
1.84 g/cc
Solids Content 31.4 %
31.4 %
by volume
61.3 %
61.3 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 500 - 1000 cP
500 - 1000 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
80.8 microns
3.18 mil
estimated wet film thickness
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 871 °C
1600 °F
Continuous
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Dry Time >= 0.25 hour
>= 0.25 hour
Recoat
0.5 hour
0.5 hour
Touch
1 hour
1 hour
Handling
Cure Time 30.0 min
0.500 hour
Air Set prior to curing
15.0 min

@Temperature 899 °C
0.250 hour

@Temperature 1650 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color White
Dry Film Coverage ft2/gal 504
at 1 mil
Thinner Water