Material Notes:
Fluoroelastomer 931 performs well in aggressive chemical where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 931 has a good field performance history in both dynamic and static applications. Fluoroelastomer 931 is excellent for high sealing load designs.Applications:Chamber sealsBonded slit valve doorsWindow sealsDoor sealsLid sealsGas inlet sealsKF fitting sealsValve sealsGasketsFitting and union sealsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.84 g/cc
1.84 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 15.48 MPa
2245 psi
ASTM D1414
Tensile Strength, Yield 6.45 MPa
936 psi
@50% Elongation; ASTM D1414
11.20 MPa
1625 psi
@100% Elongation; ASTM D1414
Elongation at Break 144 %
144 %
ASTM D1414
Compression Set 27 %
27 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Black