Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond MB600G Aqueous Based Electrically Conductive Sodium Silicate Coating

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MB600G Aqueous Based Electrically Conductive Sodium Silicate Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond MB600G is an aqueous based, sodium silicate system with graphite filler. It is intended for use in applications where moderate shielding effectiveness is required and cost is a more significant consideration. Electromagnetic interference (EMI) and radio frequency interference (RFI) are very important factors in electronic applications. The energy emitted from various sources such as radios, appliances, etc. can interfere with other electronic devices that are made from plastics. Conductive coatings are often applied to the housings in order to protect the devices from these types of interferences. Key Features Very consistent shielding effectiveness throughout the GHz regionTemperature resistance up to +700°FEasy applicationSilver coated nickel fillerHighly cost effectiveInformation provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
Solids Content 90 %
90 %
by weight
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 371 °C
700 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Electrical Properties Metric English Comments
Surface Resistance 1 - 10 ohm
1 - 10 ohm
Shielding Effectiveness 30 - 50 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
30 - 50 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
35 - 45 dB

@Frequency 2.00e+9 - 1.50e+10 Hz
35 - 45 dB

@Frequency 2.00e+9 - 1.50e+10 Hz
40 - 45 dB

@Frequency 1.50e+10 - 1.80e+10 Hz
40 - 45 dB

@Frequency 1.50e+10 - 1.80e+10 Hz
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature >=79.4 °C
1.00 - 2.00 hour

@Temperature >=175 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers