Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.46 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.46 g/cc
1.44 - 1.46 g/cc
Michelman® HydroGrease White™ 22 White coating
Description: High performance water and grease resistant white coatingUsage: HydroGrease Whiteâ„¢ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is..
Specific Gravity 1.40 - 1.46 g/cc
1.40 - 1.46 g/cc
NBR NM-IEC 60811-1-3
Karina 34/39-FC-LMP (SDB) Lilac Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.40 - 1.46 g/cc
1.40 - 1.46 g/cc
ASTM D 792
Karina E 805-02/196-CR Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.40 - 1.46 g/cc
1.40 - 1.46 g/cc
ASTM D 792
Karina E 811-10/184-Y-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.40 - 1.46 g/cc
1.40 - 1.46 g/cc
NBR NM-IEC 60811-1-1
Karina 790-38/23-CRPC Straw CPVC Compound
CPVC compound recommended for injection of fitting for use with hot water.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.42 - 1.46 g/cc
1.42 - 1.46 g/cc
ASTM D-792
Axiall 8700 Moldings & Extrusions Flexible PVC
General purpose, matte-finish extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.42 - 1.46 g/cc
1.42 - 1.46 g/cc
ASTM D-792
Axiall 9149 Wire & Cable Flexible PVC
Highly flame retardant FT-4 tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.42 - 1.46 g/cc
1.42 - 1.46 g/cc
ASTM D-792
Axiall 9149A Wire & Cable Flexible PVC
Highly flame retardant tray cable (FT-4) jacket for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.42 - 1.46 g/cc
1.42 - 1.46 g/cc
ASTM D-792
Axiall 18880 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated FT-4, tray cable jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.42 - 1.46 g/cc
1.42 - 1.46 g/cc
ASTM D-792
Axiall 8779 Moldings & Extrusions Flexible PVC
Non-lead stabilized, general purpose extrusion compound designed for PVC waterstops per Corps of Engineers Specification CRD-C 572-74.Information provided by Georgia GulfGeorgia Gulf became Axiall C..
Specific Gravity 1.40 - 1.46 g/cc
1.40 - 1.46 g/cc
NBR NM-IEC 60811-1-3
Karina 06/152-FC-LMP Blue Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Copyright © lookpolymers.com All Rights Reserved