Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)  (discontinued **)

Category Polymer , Thermoplastic , Polyamide-imide (PAI)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SINTIMID™ ESD 23 has the highest compressive strength and use temperature of the group. It is based on an Ensinger-Hyde manufactured polyamide-imide resin with a low sloughing, additive package.Information Provided by Ensinger Industries, Inc.Sintimid has been replaced with Tecasint in the Ensinger product line.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 93
93
ASTM D2240
Tensile Strength, Yield 84.8 MPa
12300 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 4.00 GPa
580 ksi
ASTM D638
Flexural Strength 134 MPa
19500 psi
ASTM D790
Compressive Strength 240 MPa
34800 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 40.5 µm/m-°C
22.5 µin/in-°F
Maximum Service Temperature, Air 313 °C
595 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+8 - 1.00e+11 ohm
1.00e+8 - 1.00e+11 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material PAI