Material Notes:
90°C rated, non-lead stabilized, inner/outer jacketing compound meets -40°C low temp impact and FT4 flame requirements in Teck 90 cables. Low acid gas 12%-13% per CSA test methods. Meets CSA 22.2 No. 131-89 Type TECK 90 Cable.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 74
68 - 74
delayed; ASTM D-2240
Tensile Strength, Yield 14.1 MPa
2050 psi
ASTM D-638
Elongation at Yield 280.7 %
280.7 %
Air Aging: 14 days @ 121°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D-746
Oxygen Index 24.5 %
24.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F