Isoflon PEEK Polyetheretherketone

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PEEK Polyetheretherketone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
DIN 53479
Water Absorption 0.50 %
0.50 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 92.0 MPa
13300 psi
DIN 53455
Elongation at Break 50 %
50 %
DIN 53455
Tensile Modulus 3.60 GPa
522 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C
26.7 µin/in-°F
DIN 52328
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 334 °C
633 °F
DIN 53736
Maximum Service Temperature, Air 250 °C
482 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Continuous; DIN 52612
Flammability, UL94 V-0

@Thickness 1.45 mm
V-0

@Thickness 0.0571 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Dielectric Constant 3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 25.0 - 30.0 kV/mm
635 - 762 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Cream
Users viewing this material also viewed the following: