Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Melt Flow 36 g/10 min

@Load 10.0 kg,
Temperature 250 °C
36 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 88.3 MPa
12800 psi
5 mm/min; ASTM D638
Flexural Strength 108 MPa
15700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 4.41 GPa
640 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.735 J/cm

@Thickness 3.17 mm
1.38 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C

@Thickness 6.40 mm
239 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 2.50 mm
V-0

@Thickness 0.0984 in