Material Notes:
Wood effect PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.13 - 1.19 g/cc
1.13 - 1.19 g/cc
ASTM D 792
ASTM Color 12.54 - 14.14
12.54 - 14.14
Color B, ME 12
15.39 - 16.99
15.39 - 16.99
Color A, ME 12
41.29 - 42.89
41.29 - 42.89
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 71 - 75

@Time 15.0 sec
71 - 75

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 24.5 MPa
>= 3560 psi
ASTM D 638
Descriptive Properties Value Comments
Application Ceiling