Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lanxess Durethan® C 38 FAM 000000 Copolyamide

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Lanxess
Trade Name Durethan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lanxess Durethan® C 38 FAM 000000 Copolyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA 6-Copolymer, non-reinforced, extrusionInformation provided by LANXESS.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Moisture Absorption at Equilibrium 3.0 %
3.0 %
50% RH; ISO 62
Water Absorption at Saturation 10 %
10 %
ISO 62
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1, -3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
cond.; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
cond.; IEC 60093
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
cond.; IEC 60250
Dielectric Strength 30.0 kV/mm

@Thickness 1.00 mm
762 kV/in

@Thickness 0.0394 in
cond.; IEC 60243-1
Processing Properties Metric English Comments
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 6 hour
2 - 6 hour
Descriptive Properties Value Comments
ISO Shortname ISO 1874 PA 6/IPDI,ES, 18-020
Users viewing this material also viewed the following: