Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Zylog Plastalloys
Trade Name Neoplast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
ASTM D 2240
59

@Time 605000 sec
59

@Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 4.90 MPa
711 psi
500 mm/min; ASTM D 412
5.49 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
797 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 360 %
360 %
500 mm/min; ASTM D 412
306 %

@Treatment Temp. 150 °C,
Time 605000 sec
306 %

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00314 GPa
0.455 ksi
500 mm/min; ASTM D 412
Tear Strength 17.7 kN/m
101 pli
500 mm/min; ASTM D 624
Compression Set 25 %

@Temperature 70.0 °C,
Time 79200 sec
25 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuous; SAE J 2236
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D 746