S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufGuard M™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.940 - 0.960 g/cc
0.940 - 0.960 g/cc
ASTM D792
Melt Flow 14.0 g/10 min
14.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 23.4 MPa
>= 3400 psi
ASTM D638
Elongation at Break >= 120 %
>= 120 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched >= 1.12 J/cm
>= 2.10 ft-lb/in
ASTM D256
Gardner Impact >= 21.7 J

@Thickness 3.17 mm
>= 16.0 ft-lb

@Thickness 0.125 in
ASTM D5420
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 3.17 mm
V-2

@Thickness 0.125 in
Oxygen Index >= 24.0 %
>= 24.0 %
ASTM D2863