Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity... |
|||
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
SCG Chemicals EL-Leneâ„¢ D682PC Low Density Polyethylene Pipe Resin Key Characteristics: High flexibility, good processingRecommended Applications: Irrigation pipesInformation provided by SCG Chemicals |
|||
Specific Gravity | 0.939 g/cc | 0.939 g/cc | ISO 1183 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |