Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A pre-colored, black homopolymer polypropylene resin specifically designed for all injection molding applications.High Flow
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648