Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Linear Mold Shrinkage, Flow | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Linear Mold Shrinkage, Flow | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.0135 cm/cm | 0.0095 - 0.0135 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latimass 52/35-04 D009 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |