LATI Latistat 62-08 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer LATI
Trade Name Latistat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latistat 62-08 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
0.0105 - 0.0135 in/in
Linear Mold Shrinkage, Transverse 0.0115 - 0.014 cm/cm
0.0115 - 0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 2.5 %
2.5 %
Tensile Modulus 3.60 GPa
522 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Vicat Softening Point 205 °C

@Load 5.00 kg
401 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 2.00e+8 ohm
2.00e+8 ohm
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 90.0 - 100 °C

@Time 10800 sec
194 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa