Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0029 cm/cm @Time 86400 sec |
0.0029 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | 60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific) LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t.. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | ISO 294 |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | ISO 294 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Linear Mold Shrinkage, Flow | 0.0029 cm/cm | 0.0029 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |
|||
Linear Mold Shrinkage, Flow | 0.0029 - 0.0049 cm/cm @Time 86400 sec |
0.0029 - 0.0049 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |