Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET)
Manufacturer BASF
Trade Name Ultradur B
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
DIN 53495/1L
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C/50% R.H.
Viscosity Test 80 cm³/g
80 cm³/g
Viscosity number
Linear Mold Shrinkage, Flow 0.0029 cm/cm
0.0029 in/in
ISO 294
Linear Mold Shrinkage, Transverse 0.0097 cm/cm
0.0097 in/in
ISO 294
Melt Flow 53.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
53.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 140 MPa
20300 psi
50mm/min; ISO 527-2
Elongation at Break 2.1 %
2.1 %
50mm/min; ISO 527
Modulus of Elasticity 10.5 GPa
1520 ksi
ISO 527-2
Charpy Impact Unnotched 4.80 J/cm²
22.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 - 225 °C
428 - 437 °F
Maximum Service Temperature, Air 210 °C
410 °F
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75
Flammability, UL94 HB

@Thickness 40.6 mm
HB

@Thickness 1.60 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Comparative Tracking Index 225 V
225 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 250 - 275 °C
482 - 527 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Descriptive Properties Value Comments
Color BK15029
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding