Physical Properties Metric English Comments
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Alcoa KAMA 4100 Prime APET  (discontinued **)
CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Alcoa KAMA Petwich-PET 4300 Petwich-PET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi..
Linear Mold Shrinkage 0.012 - 0.050 cm/cm
0.012 - 0.050 in/in
ASTM D955
Cheng Yu Plastic PP222 Flame Retardant Polypropylene, High Impact
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail en..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON F-104 PTFE Fine Powder
Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON F-205 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON F-302 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by ..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into ..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder
20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder
15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder
15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder
30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder
25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Linear Mold Shrinkage 0.010 - 0.050 cm/cm
0.010 - 0.050 in/in
0.125 in; ASTM D955
Entec Hypel® PELD20/.920 LDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Ex-Tech Plastics VersaTech™ APET
Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder
25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Alcoa KAMA 4203 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a..
Copyright © lookpolymers.com All Rights Reserved