Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® R180A Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® R180A Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Tensile Strength 24.5 MPa
3560 psi
ASTM D412
Tensile Strength, Yield 4.90 MPa
711 psi
at 100% elongation; ASTM D412
7.85 MPa
1140 psi
at 300% elongation; ASTM D412
Elongation at Break 790 %
790 %
ASTM D412
Tear Strength 78.5 kN/m
448 pli
Die C; ASTM D624
Abrasion 35
35
mm<sup>3</sup> loss; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 82.0 °C
180 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved